One-Component Flexible Composite Waterproofing Slurry
- Crack-bridging
- Easy to apply
- Crack-free curing
- Waterproof and vapor-permeable when cured
- Frost- and aging-resistant when cured
- Suitable for indoor and outdoor applications
- Tested according to the latest guidelines for issuing a general building inspection certificate (ABP) in combination with ceramic coverings, February 2008
Standards and Testing
- General building inspection certificate for waterproofing in combination with tiles and slab coverings
- Meets stress classes A1, A2, and B according to abP
- Meets moisture stress classes 0, A01, A02, and B0 according to ZDB guidelines
Application Areas
- Flexible composite waterproofing under ceramic coverings on balconies and terraces with a slope > 1%
- Flexible composite waterproofing under ceramic coverings in wet rooms, bathrooms, and steam saunas
- Structural waterproofing on basement exterior walls and retaining walls
- Sealing of swimming pools and water tanks made of solid construction. Approved up to 4 m water depth according to current test principles
- Suitable for substrates with sufficient strength such as screed, heated screed, concrete, masonry, aerated concrete, and plaster of mortar groups II and III
- For highly water-stressed areas according to stress classes A1, A2, and B of the building regulations list
- Only to be used for waterproofing from the positive side
Substrate Preparation
The substrate must be solid, load-bearing, absorbent, and largely even. Contaminants such as oil, grease, or other separating agents must be removed. Cavities and unevenness exceeding DIN 18202 tolerances must be leveled with suitable concrete filler. Pre-wet the substrate thoroughly before applying the slurry. The surface should be matt damp. Residual moisture must not exceed:
- Cement screed: 2.0%
- Anhydrite screed: 0.5%
- Heated anhydrite screed: 0.3%
Consumption
Approx. 1.4 kg/m² per mm layer thickness
Processing
To avoid lump formation during mixing, add approx. 2/3 of the required water first and mix with a suitable basket mixer at approx. 600 rpm. Add the remaining water after the material has opened. Mix for approx. 3 minutes, allow to mature briefly, then remix. Use the prepared material within one hour. Do not rework stiffened material with water. Apply the slurry with a stiff brush, trowel, or suitable spray device in 2–3 coats evenly. Maximum layer thickness: 5 mm. For tile installation in thick-bed method: apply a splatter coat into the second fresh layer. After curing, tiles can be laid in the thick-bed method.
Subsequent Work
Protect fresh waterproofing for at least 3 days from direct sunlight, rapid water loss, extreme heat, drafts, frost, and rain. After approx. 24 h, ceramic coverings can be laid with solvent-free thin-bed adhesives. For outdoor work, coverings must be void-free. Waterproofing must be fully dried before applying protective layers or backfilling (1–3 days depending on temperature and humidity). Ensure no water-retaining soil contacts the waterproofing surface. In such cases, place a 50 cm wide zone of permeable fill material in layers. Coating must be sufficiently cured (7 days) and protected (e.g., gypsum-free plaster, protective boards). Avoid point or line loads. Clean tools and contaminated areas immediately with water. Due to many possible influences, a test application is recommended. Observe the expiration date on the packaging.
Packaging
20 kg bag